materials-finishes

Austenitic Stainless Steel SUS304 vs SUS316 Pin Chambers in Salt Spray

Engineering Overview: Metallurgical comparison of SUS304 and SUS316 stainless steel lock components under ASTM B117 neutral salt spray testing.

Technical & Engineering Specifications

Molybdenum 0.0% (SUS304) vs 2.0-3.0% Mo (SUS316)
PREN Index 18.0 (SUS304) vs 24.5 (SUS316)
Salt Fog Life 480h (SUS304) vs 1000h+ (SUS316)
Alloys Compared SUS304 (1.4301) vs SUS316 (1.4401)

Stainless Steel Alloy Selection

  • SUS304 (1.4301): 18% Cr, 8% Ni. Excellent baseline corrosion resistance, but susceptible to pitting in coastal marine air.
  • SUS316 (1.4401): Incorporates 2.5% Molybdenum (Mo), boosting PREN to $\ge 24$ and surviving $>1000\text{ hours}$ salt fog.

Frequently Asked Engineering & Selection Questions

Q1: What are the primary material characteristics of this finish?

Metallurgical comparison of SUS304 and SUS316 stainless steel lock components under ASTM B117 neutral salt spray testing.