materials-finishes

ASTM B117 1000-Hour Salt Spray Testing of PVD Titanium Thin Films

Engineering Overview: Technical comparison of ASTM B117 salt fog endurance: evaluating 240h electroplated Chrome against 1000h+ vacuum PVD titanium coatings.

Technical & Engineering Specifications

PVD Ceramic > 1000 Hours (EN 1670 Grade 5)
Salt Solution 5% NaCl Salt Fog at 35°C Continuous
Testing Standard ASTM B117 / EN 1670 Corrosion Standards
Electroplated Chrome 240 - 480 Hours (EN 1670 Grade 4)

Accelerated Salt Fog Performance

In architectural door hardware, corrosion performance is quantified via continuous ASTM B117 Neutral Salt Spray (NSS) chamber exposure:

  • Galvanic Chrome: Micro-porosities pit after 240 to 480 hours.
  • PVD Ceramic (TiN/ZrN): Survives $>1000\text{ hours}$ (EN 1670 Grade 5) with zero corrosion.

Frequently Asked Engineering & Selection Questions

Q1: What are the primary material characteristics of this finish?

Technical comparison of ASTM B117 salt fog endurance: evaluating 240h electroplated Chrome against 1000h+ vacuum PVD titanium coatings.